Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon + PTFE Filled
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 117 MPa
17000 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Flexural Yield Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.59 mm
V-1

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 100 ohm-cm
10.0 - 100 ohm-cm
ASTM C611
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm
ASTM D257