Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding 50% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | |
TriStar TriSteel PE Metal Backed PTFE Bearing System Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environ.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer |
|||
Flexural Modulus | >= 13.8 GPa | >= 2000 ksi | |
Bulk Molding Compounds BMC 845 30% Glass Filled Vinyl Ester BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at .. |
|||
Flexural Modulus | 13.8 - 15.9 GPa | 2000 - 2300 ksi | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-1305/40 NAT PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 E CF20 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Conductive Appearance: Natural ColorProcessing Method: ExtrusionInformation p.. |