Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® ABS GF15 A1 15% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS GF15 A1 15% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.8 MPa
13600 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
218 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: