Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 34.2 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® TPX-HTN-01045 A 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Temperature Stre.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS WM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ASA GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ASA GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE 0226 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE E GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: .. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0096 S LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0112 B AM2 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Antimicrobial (Fungicide)Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0142 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0225 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6 SF76 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (76%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6 SF80 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP 0112 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPX-HTN-01092 A 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ABS GF15 A1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GFB20 20% Glass/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabiliz.. |