Techmer ES HiFill® ABS GF60 60% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS GF60 60% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Thickness 3.17 mm
0.00050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 12.8 GPa
1850 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB