Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.8 GPa | 1860 ksi | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla.. |
|||
Flexural Modulus | 12.8 GPa @Temperature 23.0 °C |
1860 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B11^ F45 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 12.8 GPa @Temperature 23.0 °C |
1860 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B12^ F45 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | 5 mm/min; ISO 178 |
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Silicone LubricantFeatures: Lubricated, Low Friction and Good Wear .. |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced |
|||
Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ASTM D790 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ASTM D790 |
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive) Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resist.. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ASMT D790 |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ISO 178 |
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ISO Data |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Flexural Modulus | 12.8 - 13.6 GPa | 1860 - 1970 ksi | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |
|||
Flexural Modulus | 12.8 GPa | 1860 ksi | ASTM D790 |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |