Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 141 MPa
20400 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 8.69 GPa
1260 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
0.854 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
10.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 257 °C
495 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Strength 20.5 kV/mm
520 kV/in
Method A (Short-Time); ASTM D149