Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IPC-TM-650.2.5.17 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | IEC 60093 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | IEC 60093 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
PolyOne Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+13 - 4.00e+16 ohm | 1.00e+13 - 4.00e+16 ohm | Average value: 5.09e+15 ohm Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | |
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
LATI Latigray 47/1-01 CX/45 PP Copolymer Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 93 |
Solvay Technyl® C 206 Nylon 6, EH0 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257, IEC 93 |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled Information provided by Adamas, HPM |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | Conditioned; CEI 60093 |
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact PBT+PCInformation provided by BARLOG plastics GmbH. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
CENTROPLAST CENTROPEEK Polyetheretherketone This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | dry; IEC 60093 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | E - 24/125; IPC-TM-650.2.5.17.1 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Surface Resistance | 1.00e+13 - 7.30e+17 ohm | 1.00e+13 - 7.30e+17 ohm | Average value: 8.24e+16 ohm Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+17 ohm | 1.00e+13 - 1.00e+17 ohm | Average value: 5.27e+16 ohm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |