Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 2.01 g/cc
0.0726 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
345 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
ASTM D257
Users viewing this material also viewed the following: