Polymer Property : Flexural Modulus = 5.65 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.65 GPa
820 ksi
Tangent; ASTM D790
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Flexural Modulus 5.65 GPa
819 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC (Asia Pacific)
LNP* Lubriloy* DF2049 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant.
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Techmer ES Electrablend® PC SS15 FR BK 15% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr..
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T..
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Techmer ES HiFill® PA6/6 CM40 6122 BK 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: Injection Mol..
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF/B40 L 20% Glass Bead/Glass Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation ..
Flexural Modulus 5.65 GPa
819 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC
LNP* THERMOCOMP* DX06411 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Flexural Modulus 5.65 GPa
819 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC (Asia Pacific)
LNP* Thermocomp* DX06411 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 5.65 GPa
819 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp JF003L PES
LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r..
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned
Property data is for samples at equilibrium moisture (0.7%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo..
Flexural Modulus 5.65 GPa
819 ksi
ISO 178
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
Copyright © lookpolymers.com All Rights Reserved