Material Notes:
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 2.8 %

@Time 86400 sec
2.8 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D638
Elongation at Break 85 %
85 %
ASTM D638
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm

@Thickness 3.17 mm
3.30 ft-lb/in

@Thickness 0.125 in
ASTM D256