Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA6 L UV (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 L UV (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 2.8 %

@Time 86400 sec
2.8 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 95 %
95 %
ASTM D638
Flexural Strength 41.4 MPa
6000 psi
ASTM D790
Flexural Modulus 0.738 GPa
107 ksi
ASTM D790
Izod Impact, Notched >= 8.54 J/cm

@Thickness 3.17 mm
>= 16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Users viewing this material also viewed the following: