Material Notes:
Availability: North AmericaForms: PelletsFeatures: Copolymer and Thermally ConductiveInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 20.7 MPa
3000 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Thermal Conductivity 1.30 W/m-K
9.00 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C
175 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 11.8 kV/mm
300 kV/in
Method A (Short-Time); ASTM D149