Techmer ES HiFill® TPU 0445 A

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® TPU 0445 A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 4.45 g/cc
0.161 lb/in³
ASTM D792
Water Absorption 0.025 %

@Time 86400 sec
0.025 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 57
57
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Flexural Modulus 0.241 GPa
35.0 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM D648