Techmer ES Luriblend® HTN 01420 BK

Category Polymer , Thermoplastic , Nylon , High Temperature Nylon
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® HTN 01420 BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.27 %

@Time 86400 sec
0.27 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Yield Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.8 µm/m-°C
26.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
298 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB