Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® TPU T/AL27 Aramid Fiber Filled

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® TPU T/AL27 Aramid Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber FilledAdditive: PTFE LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Elongation at Yield 100 %
100 %
ASTM D638
Flexural Yield Strength 62.7 MPa
9100 psi
ASTM D790
Flexural Modulus 0.276 GPa
40.0 ksi
ASTM D790
Izod Impact, Notched 2.19 J/cm

@Thickness 3.17 mm
4.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
429 °F