Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet) |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Quantum PVDF Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
I. Stern 728 High Gloss Medium Natural ABS Features:Super high glossEasy to colorApplicationsInjection moldingAppliancesInformation provided by I. Stern & Co. Inc. |
|||
Tensile Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | ASTM D638 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Shuman 310 Utility Black PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Shuman 330 White PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Shuman 380 Grey PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D412 |
Teknor Apex Laripur® LPR 9060EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Luriblend® TPU T/AL27 Aramid Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber FilledAdditive: PTFE LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638, ASTM D1708 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Tensile Strength | 48.3 MPa | 7010 psi | ASTM D412 |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, .. |
|||
Tensile Strength | 48.3 MPa | 7010 psi | ASTM D412 |
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Tensile Strength | >= 48.3 MPa | >= 7000 psi | |
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | Cross; IPC TM-650 2.4.18.3 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon CLTE-AT Commercial Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | Cross; ASTM D882 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
Tensile Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Tensile Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Tensile Strength | 48.3 MPa | 7000 psi | ASTM D638 |
Aaron Industries AAROPRENE® AE PC/ABS 7000-1 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Tensile Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Tensile Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Tensile Strength | 48.3 MPa | 7010 psi | ASTM D412 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Tensile Strength | 48.3 MPa @Temperature 75.0 °C, Time 0.000 sec |
7010 psi @Temperature 167 °F, Time 0.000 hour |
30 Mil Sheet, Immersion in Water |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Tensile Strength | 48.3 MPa | 7010 psi | ASTM D412 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |