Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® J-50/30/TF/10 Polycarbonate, 30% GFR, 10% PTFE

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass + PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-50/30/TF/10 Polycarbonate, 30% GFR, 10% PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslube glass fiber reinforced polytetrafluorethylene (PTFE) lubricated polycarbonate grades have an excellent balance of mechanical strength characteristics, dimensional stability and wear and friction performance. These products are ideal candidates for gears and gear trains, as well as wear pads and bearings. The proprietary PTFE and polymer lubricant blend lubricated grades add additional cost/performance versus traditional PTFE lubricated polycarbonate compounds.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Water Absorption 0.090 %
0.090 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 124 MPa
18000 psi
ASTM D638
Flexural Yield Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256