Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
24 Hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527
Elongation at Break 18 %
18 %
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 4.60 kJ/m²
2.19 ft-lb/in²
ISO 180/1A