Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.60 - 6.00 kJ/m² | 2.19 - 2.86 ft-lb/in² | Average value: 5.53 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched (ISO) | 4.60 - 9.70 kJ/m² @Temperature -40.0 - -40.0 °C |
2.19 - 4.62 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 6.98 kJ/m² Grade Count:5 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 4.60 kJ/m² | 2.19 ft-lb/in² | ISO 180/1A |
Techmer ES Plaslube® NY-6/MS/M PA12 |
|||
Izod Impact, Notched (ISO) | 4.60 kJ/m² | 2.19 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Izod Impact, Notched (ISO) | 4.60 kJ/m² | 2.19 ft-lb/in² | ISO Test |
BASF Ultramid® B3GM35 Ebony23227 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 Ebony23227 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Izod Impact, Notched (ISO) | 4.60 - 16.0 kJ/m² @Temperature -40.0 - -20.0 °C |
2.19 - 7.61 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 8.37 kJ/m² Grade Count:15 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |