Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 2.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 43.4 MPa
6300 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 73.8 MPa
10700 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm

@Thickness 3.17 mm
2.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: