Material Notes:
Notes: 75°C Insulation; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 85
85
10 seconds; ASTM D2240
Tensile Strength at Break 14.8 MPa
2150 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 27 %
27 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 9.90e+12 ohm-cm
9.90e+12 ohm-cm
ASTM D257
Dielectric Constant 3.56

@Frequency 1.00e+6 Hz
3.56

@Frequency 1.00e+6 Hz
ASTM D150
5.12

@Frequency 1000 Hz
5.12

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.065

@Frequency 1.00e+6 Hz
0.065

@Frequency 1.00e+6 Hz
ASTM D150
0.073

@Frequency 1000 Hz
0.073

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: