Material Notes:
Forms: Pellets Additional Information: HDT, Unannealed; 264 psi, 0.125 in bars: 66.4°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
10 seconds; ASTM D2240
Tensile Strength at Break 43.6 MPa
6330 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Izod Impact, Notched 7.47 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
14.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 118 J/cm

@Thickness 12.7 mm,
Temperature 22.8 °C
0.221 ft-lb/mil

@Thickness 0.500 in,
Temperature 73.0 °F
Procedure A
Descriptive Properties Value Comments
Appearance Opaque