Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.48 GPa | 360 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Tensile Modulus | 2.48 - 2.69 GPa | 360 - 390 ksi | ASTM D638 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)
(discontinued **) Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | |
Ineos ABS Lustran® 446 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ISO 527-2/50; ASTM D638 |
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |
|||
Tensile Modulus | 2.48 GPa @Temperature 22.8 °C |
360 ksi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall 9109J Clear Rigid PVC, Extrusion, Clear Georgia Gulf 9109J Clear is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer, which retards color change.Information provided by Georgia GulfGeo.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall SP-7008 Rigid PVC, Molding Georgia Gulf SP-7008 is a rigid vinyl compound formulated for electrical fittings and molded parts requiring high impact strength and toughness.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall 8258 Rigid PVC, Extrusion Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall 9113 White 02 Rigid PVC, Molding, White 02 Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |