Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
10 seconds; ASTM D2240
Tensile Strength at Break 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 56 %
56 %
ASTM D638
Tensile Modulus 2.75 GPa
399 ksi
ASTM D638
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 97.7 J/cm
0.183 ft-lb/mil
Procedure A
Descriptive Properties Value Comments
Appearance Opaque