Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications.
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl TN240 PPE+PS
PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t..
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific)
PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL TN300 PPE+PS
PPE+PS. Transparent. High heat. Color Limited. Injection molding. Laser-Transmission welding applications.
Flexural Modulus 2.82 GPa
409 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66
LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubriloy D20001 PC
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by..
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009P PC
LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing, Flame Retardant...
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific)
LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific)
LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*..
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX03571 PC
LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Flexural Modulus 2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX03571 PC
LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP
LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid
Forms: PelletsInformation Provided by Teknor Apex
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific)
LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber.
Flexural Modulus 2.82 GPa
409 ksi
ASTM D-790
Axiall LSS-8200 Rigid PVC, Extrusion
Georgia Gulf LSS-8200 is a special purpose rigid PVC sheet extrusion compound designated for reduced smoke emission properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..