Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Fireguard® 910-LBF Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Fireguard®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Fireguard® 910-LBF Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RoHS Compliant Features: Bromine Free; Flame Retardant; Low Smoke Emission Uses: Insulation; Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 1651; UL 444; UL QMTT2 .E200337 Processing Method: Extrusion Forms: Pellets Additional Information: Cone Calorimeter, Peak Heat Release Rate: 106 kW/m2 Cone Calorimeter, Average Heat Release Rate: 59 kW/m2 Cone Calorimeter, Total Heat Released: 70 MJ/m2 Cone Calorimeter, Average Specific Extinction Area: 348 m2/kg Peak Smoke: 2 1/m Dynamic Heat Stability at 205°F, 100 RPM, 72 gr. #5 Bowl: 37 min to decomposition Kayeness ACR at 350°F: 271 Pa-sInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 87
87
10 seconds; ASTM D2240
92
92
ASTM D2240
Tensile Strength at Break 17.7 MPa
2570 psi
ASTM D638
Elongation at Break 190 %
190 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -5.00 °C
23.0 °F
ASTM D746
Oxygen Index 43 %
43 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.49

@Frequency 1.00e+6 Hz
3.49

@Frequency 1.00e+6 Hz
ASTM D150
4.47

@Frequency 1000 Hz
4.47

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.033

@Frequency 1.00e+6 Hz
0.033

@Frequency 1.00e+6 Hz
ASTM D150
0.072

@Frequency 1000 Hz
0.072

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 196 °C
385 °F
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: