Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.7 MPa | 2570 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3782 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D638 |
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin
(discontinued **) MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle.. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D412 |
Teknor Apex APEX® 3085-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D638 |
Teknor Apex Fireguard® 910-LBF Polyvinyl Chloride, Flexible RoHS Compliant Features: Bromine Free; Flame Retardant; Low Smoke Emission Uses: Insulation; Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC.. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D412 |
Teknor Apex APEX® 2080-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D412 |
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D3759 |
3M 767 Hazard Marking Vinyl Tape 3M™ Hazard Marking Vinyl Tape 767 can be used in safety applications.Information provided by 3M |
|||
Tensile Strength at Break | 17.7 MPa | 2570 psi | ASTM D638 |
Asahi Glass AFLAS® 150P TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |