Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (430000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Molding; Extrusion; Injection Molding; Film Extrusion Additional Information: Recommended Dosage: 2.5-5.0%Information Provided by Teknor Apex
Physical Properties Metric English Comments
Melt Flow 5.00 g/10 min

@Load 10.0 kg,
Temperature 190 °C
5.00 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Descriptive Properties Value Comments
Appearance Black