Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ter Hell Plastic Terez® PA 6 7500 GF 30 Polyamide 6, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PA 6 7500 GF 30 Polyamide 6, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Medium viscosity Polyamide 6, 30% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with good stiffness and good impact resistance.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Water Absorption 6.3 %
6.3 %
ISO 62
Moisture Absorption at Equilibrium 1.9 %
1.9 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 180 MPa
26100 psi
dry; ISO 527
Tensile Strength, Yield 180 MPa
26100 psi
dry; ISO 527
Elongation at Break 4.0 %
4.0 %
dry; ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
dry; ISO 527
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
dry; ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 60695
Electrical Properties Metric English Comments
Comparative Tracking Index 550 V
550 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 240 - 270 °C
464 - 518 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour