Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, Conditioned Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-23H PA12-GF23 Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |