Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Dry impact unfilled Polyamide 6.6, good flowability and demolding properties.Application: Molding parts of different kinds, high impact properties.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Water Absorption 7.5 %
7.5 %
ISO 62
Moisture Absorption at Equilibrium 2.1 %
2.1 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 60.0 MPa
8700 psi
dry; ISO 527
Tensile Strength, Yield 75.0 MPa
10900 psi
dry; ISO 527
Elongation at Break 30 %
30 %
dry; ISO 527
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527
Tensile Modulus 2.80 GPa
406 ksi
dry; ISO 527
Charpy Impact Unnotched NB
NB
dry; ISO 179
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 2 - 4 hour
2 - 4 hour
Users viewing this material also viewed the following: