Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® CR 7228 - 30% Talc/Mineral Reinforced Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® CR 7228 - 30% Talc/Mineral Reinforced Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Mineral Reinforced PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break >= 25 %
>= 25 %
ASTM D638
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
ASTM D648