Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® SEB 200 - 20% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® SEB 200 - 20% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 80.0 MPa
11600 psi
ASTM D638
Elongation at Break >= 6.0 %
>= 6.0 %
ASTM D638
Flexural Yield Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
ASTM D790
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
ASTM D648