Total HDPE 2008 SN 60 High Density Polyethylene - Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE 2008 SN 60 High Density Polyethylene - Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE 2008 SN 60 is a high density polyethylene with very high stiffness and low viscosity. It has been specifically designed for the manufacture of thin walled containers for foodstuffs.HDPE 2008 SN 60 is a pellet grade and contains antioxidants.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.961 g/cc
0.961 g/cc
ISO 1183
Environmental Stress Crack Resistance 10 hour
10 hour
F50, Anatarox 100%; ASTM D 1693/B
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
52 g/10 min

@Load 21.6 kg,
Temperature 190 °C
52 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179-1
Processing Properties Metric English Comments
Processing Temperature 180 - 220 °C
356 - 428 °F