Total Lacqrene® 4431 Flame Retardant Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqrene® 4431 Flame Retardant Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQRENE ® 4240 is a high impact, flame retardant polystyrene with excellent thermal stability.ApplicationTelevision back coversInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D1505
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238G
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.6 MPa
3270 psi
ASTM D638M
Elongation at Break 50 %
50 %
ASTM D638M
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
50N; ASTM D1525B
95.0 °C
203 °F
10N; ASTM D1525A
Processing Properties Metric English Comments
Processing Temperature <= 240 °C
<= 464 °F
Users viewing this material also viewed the following: