Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lacqrene® 814(EU) High Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqrene® 814(EU) High Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQRENE® 814 is a PBDE free high impact, flame retardant polystyrene with excellent UV stability, rated UL 94 V0 @ 2mm and UL 94 5 VA @ 3mm.ApplicationCovers for electrical equipment, External covers for office equipment, TV back covers, Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 MPa
2760 psi
ISO 527-2
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 572-2
Elongation at Break 45 %
45 %
ISO 527-2
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
50N (T° increase = 5°C/h); ISO 306B50
97.0 °C
207 °F
10N (T° increase = 50°C/h); ISO 306A50
Processing Properties Metric English Comments
Processing Temperature <= 240 °C
<= 464 °F
Users viewing this material also viewed the following: