Total Lacqtene® 1003 FE 30 HDPE, blow molding  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 1003 FE 30 HDPE, blow molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium density radical polyethylene made by high tubular pressure process for medical applications requiring sterilization : small and medium stiff containers for parental mixtures, ophthalmic solutions, sterilized ampoules.Advised temperature profile : 150 to 180°C Lacqtène 1003FE30 is easily converted on aseptical machines. (Rommelag or similar)Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min
0.30 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527
Elongation at Break 550 %
550 %
ISO 527
Modulus of Elasticity 0.350 GPa
50.8 ksi
ISO 527-2
Dart Drop Test 150 g
0.331 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 117 °C
243 °F
ISO 11357-3
Vicat Softening Point 106 °C
223 °F
ISO 306
Optical Properties Metric English Comments
Haze 10 %
10 %
50µ; ASTM D 1003
Descriptive Properties Value Comments
Food Status This material complies with the French and European pharmacopeas.