Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® MR30MC2 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection molding. Lumicene® MR30MC2 differs from the other random copolymers by its molding reproducibility, outstanding organoleptic properties combined with low extractables, excellent transparency and gloss.Producers of rigid food packaging, caps and closures, medical device and packaging, housewares and kitchenware will take full advantage of the new Lumicene® random metallocene product range.Peroxide is not used in the manufacturing of the above mentioned product.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 30 g/10 min
30 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ISO 572-2
Elongation at Yield 10 %
10 %
ISO 572-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 572-2
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 140 °C
284 °F
ISO 3146