Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 5752 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7650 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7650 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a medium fluidity offering a combination of ease of processing and excellent impact propert.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 3150 Polypropylene, Homopolymer Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 7089 Polypropylene Homopolymer, Fiber Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9059 is homopolymer.ApplicationATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9069 is homopolymer.ApplicationATOFINA Polypropylene PPH 9069 is intended for applications in non-wovens. It is also suitable for extrusion of bulk continuous filament (BC.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion Polypropylene PPR 3221 is a high clarity, high impact resistance random copolymer especially designed for blow molding applications (mono and multi-layers) for food and non-food packaging of sauces,.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 13442 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 13442 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by very high fluidity with good mechanical properties. It has been formulated for excellent ant.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Bulk Density | 0.525 - 0.650 g/cc | 0.0190 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® UV 50 20% active PE based anti-UV masterbatch Fields of application: Foils, films, fibers, extruded and injection molded articles made from PE compatible resins.Examples: Tapes, ropes, carpets, non-wovens, films, fibers, garden furniture, autom.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |