Material Notes:
Polystyrene 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. The material demonstrates excellent strength and good temperature resistance. The varied applications include electronic packaging, extruded light diffusers and office accessories.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 106 °C
222 °F
ASTM D1525