Material Notes:
Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of thermoformed cups and containers. Other features include excellent extrusion processing, good gloss, and FDA compliance.825EX is utilized in such products as drinking cups, dairy containers, bowls, and drink lids.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Falling Dart Impact 13.6 J
10.0 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 90 %
90 %
60°; ASTM D523