Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 98.9 °C | 210 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
M. Holland Company GS411 Polystyrene
(discontinued **) Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Global D-2022 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 150 °C Grade Count:29 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
I. Stern 108B Utility Black ABS Features:Good processing characteristicsInjection Molding and ExtrusionApplicationsProfilesPicture Frames, Tubes, RodsSpools, ReelsInformation provided by I. Stern & Co. Inc. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
I. Stern 870E High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetprofilesAgency Rating.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
I. Stern BLK100 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetProfilesAgency Rating.. |
|||
Vicat Softening Point | 98.9 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Vicat Softening Point | 98.9 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 6220 HIPS Excellent toughnessHigh glossDesigned for deep draw thermoformingInformation provided by Styrolution |
|||
Vicat Softening Point | 98.9 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D648 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Total PSI 740 Polystyrene Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding. It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, suc.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Total PSI 825E Polystyrene Polystyrene 825E is a high impact polystyrene designed specifically for extrusion/thermoforming. Over the years, this popular resin has established itself as the standard extrusion grade high impact.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Total PSI 825EX Polystyrene Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Total PSI 844E Polystyrene Polystyrene 844E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough ductile sheet with a rich matte finish. 844E is specially formulated to minim.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
American Polymers API 500 Polystyrene API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
American Polymers API 545 Polystyrene API 545 is a high impact, high heat resistant grade of impact modified polystyrene. This material features fast set-up as well as easy colorability.Applications: API 545 is suggested for heavy part.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Dow 620I Linear Low Density Polyethylene (LDPE) For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als.. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Amco Amalloy® B1172 Polymer Alloy Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D1525 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D648 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, High Flow Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 154 °C Grade Count:8 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |