Total Xsene® XS10 OS HDPE, pipe

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Total Atofina
Trade Name XSene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Xsene® XS10 OS HDPE, pipe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FINATHENE® XS 10 OS is a cadmium-free orange stripe compound designed to be used in combination with the black PE 100 grade FINATHENE® XS 10 B for gas pipe application. The base polymer of FINATHENE® XS 10 OS is the same as the base polymer of FINATHENE® XS 10 B.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
200°C; EN 728
Melt Flow 0.30 g/10 min

@Load 5.00 kg
0.30 g/10 min

@Load 11.0 lb
ISO 1133