Toyobo Pelprene™ S-6001 Polyester TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer Toyobo
Trade Name Pelprene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Pelprene™ S-6001 Polyester TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block copolymer consisting of an aromatic polyester as the hard segment and an aliphatic polyester as the soft one. It has physical properties similar to the 'P' type and excellent heat aging and weather resistance.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.30 %
0.30 %
25°C; 65%RH
Linear Mold Shrinkage 0.017 cm/cm

@Thickness 2.00 mm
0.017 in/in

@Thickness 0.0787 in
Melt Flow 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 99
99
ASTM D2240
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 490 %
490 %
ASTM D638
50% Modulus 0.0275 GPa
3.99 ksi
ASMT D638
Flexural Modulus 0.570 GPa
82.7 ksi
ASTM D790
Compressive Modulus 0.0310 GPa
4.50 ksi
10% Compression Modulus; ASTM D695
Resilience 56
56
JIS K6301
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Tear Strength 196 kN/m
1120 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 8.0
8.0
CS-17 wheel; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
TMA
Melting Point 218 °C
424 °F
DSC
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ASTM D648
Vicat Softening Point 202 °C
396 °F
ASTM D1525
Brittleness Temperature -60.0 °C
-76.0 °F
JIS K6301
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Dielectric Strength 30.0 kV/mm
762 kV/in
JIS K2111