Material Notes:
TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
Cured
Water Absorption 2.7 %
2.7 %
24 hrs @ 100°C & 1.5 ATM
Viscosity 3300 cP
3300 cP
Mixed (cp #40, 2.5 rpm)
Mechanical Properties Metric English Comments
Adhesive Bond Strength 18.6 MPa
2700 psi
Lap shear, alum to alum, cured 10 min @ 140°C
Thermal Properties Metric English Comments
CTE, linear 47.0 µm/m-°C

@Temperature 10.0 - 50.0 °C
26.1 µin/in-°F

@Temperature 50.0 - 122 °F
Alpha 1
144 µm/m-°C

@Temperature 150 - 200 °C
80.0 µin/in-°F

@Temperature 302 - 392 °F
Alpha 2
Glass Transition Temp, Tg 80.0 °C
176 °F
Ultimate Tg, 10°C/min; TMA
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 140 °C
0.167 hour

@Temperature 284 °F
60.0 min

@Temperature 80.0 °C
1.00 hour

@Temperature 176 °F
Pot Life >= 480 min

@Temperature 20.0 - 22.0 °C
>= 480 min

@Temperature 68.0 - 71.6 °F
Descriptive Properties Value Comments
Color Brown
Cured
Tan
Mixed