Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste silver-filled epoxy adhesive is solvent free, does not contain any copper, nickel or carbon additives, and develops strong, durable electrically and thermally conducting bonds and seals between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TRA-DUCT 916H03 cures at room temperature, and can be used as a "cold-solder" for heat-sensitive components where hot-soldering is impractical. It can also be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 57500 cP
57500 cP
Mixed (cp #52, 5 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
2 hrs @ 65°C
Adhesive Bond Strength 4.83 MPa
700 psi
Lap shear, alum to alum, 2 hrs @ 65°C
4.83 MPa
700 psi
Lap shear, alum to alum, 24 hrs @ 25°C
10.17 MPa
1475 psi
Lap shear, alum to alum, 1 hr @ 110°C
Thermal Properties Metric English Comments
CTE, linear 42.0 µm/m-°C
23.3 µin/in-°F
Below Tg
230 µm/m-°C
128 µin/in-°F
Above Tg
Glass Transition Temp, Tg 50.0 °C
122 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.00010 ohm-cm
0.00010 ohm-cm
cured 1 hr @ 110°C
0.0010 ohm-cm
0.0010 ohm-cm
cured 2 hrs @ 65°C
0.010 ohm-cm
0.010 ohm-cm
cured 24 hrs @ 25°C
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Light Yellow
Hardener
Silver
Resin/Mixed/Cured
Thixotropic Index 3
1 rpm/10 rpm