Polymer Property : Adhesive Bond Strength = 700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.83 MPa
700 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s..
Adhesive Bond Strength 4.83 MPa
700 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s..
Adhesive Bond Strength 4.83 MPa
700 psi
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Emerson & Cuming 57C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, electrically conductive, room temperature curing, epoxy adhesive. Good thermal conduc..
Adhesive Bond Strength 4.83 MPa
700 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop..
Adhesive Bond Strength 4.83 MPa
700 psi
Adhesive tensile shear strength; ASTM D1002
Devcon Magic Bond™ Epoxy Putty
Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,..
Adhesive Bond Strength 4.83 MPa
700 psi
Cured property; Lap Shear failure in polycarbonate substrate; ASTM D1002
Aptek 2209-A/B Clear, non-yellowing urethane adhesive
APTEK 2209-A/B is a water clear, thixotropic, two component, electrically insulating, urethane adhesive designed for bonding various substrates. APTEK 2209-A/B is effective for bonding plastics and..