Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® D 778 One-Component Fast Cure Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® D 778 One-Component Fast Cure Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming D 778 Eccobond® One-Component Fast Cure Epoxy AdhesiveHigh strength, semi-flexible, thixotropic, fast heat curing, epoxy structural adhesive. Good peel strength (20 pli). Recommended for reinforcing riveted or weld bonded metal panels for cabinets, buses, trailers or other sheet metal structures. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 19.3 MPa
2800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 160 °C
0.167 hour

@Temperature 320 °F
20.0 min

@Temperature 120 °C
0.333 hour

@Temperature 248 °F
45.0 min

@Temperature 100 °C
0.750 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Color Yellow
Viscosity Thixotropic Paste
Users viewing this material also viewed the following: