Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced , Epoxy, Thermally Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in harsh environments. Typical applications include sensors, transformers, power supplies, and rectifiers.Emerson & Cuming 906-1 Stycast® One-Component Epoxy High Service Temp EncapsulantThermally ConductiveGood Chemical ResistanceFilled Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Viscosity 190000 cP

@Temperature 25.0 °C
190000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
Thermal Conductivity 0.860 W/m-K
5.97 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time >= 8.00 min
>= 0.133 hour
Users viewing this material also viewed the following: